Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 48.1 MPa @Temperature 260 °C |
6980 psi @Temperature 500 °F |
ASTM D790 |
Daelim H&L Plavis G40 Aromatic Polyimide, 40% Graphite Filled, Machined Parts Higher abrasion resistance than G15, high value stability and very low friction coefficient propertyInformation provided by Daelim H&L |