Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 65.1 MPa @Temperature 260 °C |
9440 psi @Temperature 500 °F |
ASTM D790 |
Daelim H&L Plavis N Aromatic Polyimide, Non-Filled, Machined Parts Superior chemical property, very high radiation resistance, electrical and thermal property, low outgassing and superior physical propertyInformation provided by Daelim H&L |