Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 600 MPa @Temperature 23.9 °C |
87000 psi @Temperature 75.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® P-670I Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-670I is a versatile, non-styrenated/low VOC polyester resin. P670I is used in a wide variety of applications including radomes, tooling and aircraft structures.Key Features and Benefits:.. |