Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 52.0 MPa @Temperature 260 °C |
7540 psi @Temperature 500 °F |
ASTM D790 |
Daelim H&L Plavis N Aromatic Polyimide, Non-Filled, Direct Formed
(Unverified Data**) Information provided by Daelim H&L |