Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 503 MPa @Temperature -53.9 °C |
73000 psi @Temperature -65.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 285 Kevlar® Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |