Polymer Property : Flexural Strength = 496 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 496 MPa

@Temperature 21.1 °C
72000 psi

@Temperature 70.0 °F
Wet; ASTM D790
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Flexural Strength 496 MPa

@Temperature 23.9 °C
72000 psi

@Temperature 75.0 °F
Dry; ASTM D790
Park Electrochemical Nelcote® P-650M Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-650M is a polyester resin system suitable for coating on any MIL-C-9084. P-650M has good electrical and mechanical properties and has been used in a wide variety of applications, includi..
Flexural Strength 496 MPa

@Temperature 71.1 °C
72000 psi

@Temperature 160 °F
Dry; ASTM D790
Park Electrochemical Nelcote® P-650R Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-650R is a non-styrenated/low VOC polyester resin system that has been designed for optical clarity. P-650 exhibits good mechanical properties up to 250°F.Key Features and Benefits:Non-s..