Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 337 MPa @Temperature -40.0 °C |
48900 psi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-665C30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |