Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 3.28 MPa @Strain 30.0 % |
475 psi @Strain 30.0 % |
Load applied normal to fiber plane, strain = load deformation in mils; Three point bending, sample 0.5"*0.5"*4" |
Zircar Ceramics AL-30 Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Flexural Strength | 3.28 MPa @Strain 35.0 % |
475 psi @Strain 35.0 % |
Load applied parallel to fiber plane, strain = load deformation in mils; Three point bending, sample 0.5"*0.5"*4" |
Zircar Ceramics AL-30 Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |