Polymer Property : Flexural Strength = 461 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 461 MPa

@Thickness 1.57 mm
66800 psi

@Thickness 0.0620 in
LW
Industrial Laminates/Norplex NP190 Synthetic Fabric  (discontinued **)
Description: Aramid fabric material with a high performance phenolic resin matrix. Excellent electrical and mechanical properties at elevated temperatures, and in adverse environments. Applications ..