Mechanical Properties Metric English Comments
Flexural Strength 308 MPa

@Thickness 1.57 mm
44600 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP634 Laminate
Description: Warm punching, composite grade with woven glass covers for improved flexural, tensile and impact strength. Electrical properties comparable to NP611.Thickness Tested: 0.062", 0.125" and..