Mechanical Properties Metric English Comments
Flexural Strength 265 MPa

@Temperature 125 °C
38400 psi

@Temperature 257 °F
ISO 178
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com..