Flexural Strength 365 MPa

@Strain 3.00 %
52900 psi

@Strain 3.00 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 50% glass fibers, injection moldingInformation provided by LANXESS.