Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 359 MPa @Temperature 121 °C |
52000 psi @Temperature 250 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® P-650M Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-650M is a polyester resin system suitable for coating on any MIL-C-9084. P-650M has good electrical and mechanical properties and has been used in a wide variety of applications, includi.. |
|||
Flexural Strength | 359 MPa @Thickness 1.57 mm |
52000 psi @Thickness 0.0620 in |
CW; ASTM D790 |
Industrial Laminates/Norplex NP510A Glass Fabric Description: Woven glass fabric epoxy laminate. Engineered to provide NEMA grade FR-4 properties. This material contains bromine on the epoxy resin backbone. Certifiable to MIL-I-24768/27, Type GEE-.. |