Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 153 MPa @Temperature -40.0 °C |
22200 psi @Temperature -40.0 °F |
Practical Use; ASTM-D790 |
Toyobo GLAMIDE® TY-835TC Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |