Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1520 MPa @# of Cycles 330000 |
220000 psi @# of Cycles 330000 |
|
QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core Description: Ferrium® C64™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the .. |
|||
Flexural Strength | 1520 MPa @# of Cycles 550000 |
220000 psi @# of Cycles 550000 |
|
QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core Description: Ferrium® C64™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the .. |
|||
Flexural Strength | 1520 MPa @# of Cycles 1.20e+6 |
220000 psi @# of Cycles 1.20e+6 |
|
QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core Description: Ferrium® C64™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the .. |