Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1830 MPa @# of Cycles 49000 |
265000 psi @# of Cycles 49000 |
|
QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core Description: Ferrium® C64™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the .. |
|||
Flexural Strength | 1830 MPa @# of Cycles 80000 |
265000 psi @# of Cycles 80000 |
|
QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core Description: Ferrium® C64™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the .. |
|||
Flexural Strength | 1830 MPa @# of Cycles 100000 |
265000 psi @# of Cycles 100000 |
|
QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core Description: Ferrium® C64™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the .. |