Polymer Property : Flexural Strength = 164 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 164 MPa

@Thickness 1.57 mm
23800 psi

@Thickness 0.0620 in
LW; ASTM D790
Industrial Laminates/Norplex NP322 Cotton Fabric
Description: Linen phenolic laminate with molybdenum disulfide. Provides the same lubricity as NP313, but has better machining qualities. Mechanical strength similar to, but slightly less than NP320..