Polymer Property : Flexural Strength = 143 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 143 MPa

@Thickness 1.57 mm
20700 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP342 Cotton Fabric
Description: Fine weave canvas phenolic material with fabric construction weight intermediate to NP310 and NP320. Designed for better machining than grade NP310 and lower cost than NP320.Thickness T..