Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 139 MPa @Thickness 1.57 mm |
20100 psi @Thickness 0.0620 in |
LW; ASTM D790 |
Industrial Laminates/Norplex NP325 Cotton Fabric Description: Linen phenolic laminate with graphite added as a solid lubricant. Linen substrate provides better machining and wear resistance than NP315.Thickness Tested: 0.062", 0.125" and 0.500". |