Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 92.0 MPa @Strain 5.00 %, Temperature 23.0 °C |
13300 psi @Strain 5.00 %, Temperature 73.4 °F |
ASTM D790 |
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod.. |