Flexural Strength 128 MPa

@Thickness 1.57 mm
18500 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP320 Cotton Fabric
Description: Fine weave (less than 4 ounce/square yard) cotton fabric commonly called linen, combined with phenolic resin to provide better machining than NP310. For smaller and more intricate shape..