Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 118.5 MPa @Temperature 23.0 °C |
17190 psi @Temperature 73.4 °F |
ASTM D790 |
Daelim H&L Plavis G15 Aromatic Polyimide, 15% Graphite Filled, Machined Parts High abrasion resistance, very low friction coefficient property, suitable for being applied to spin component of spin apparatusInformation provided by Daelim H&L |