Flexural Strength 700 - 900 MPa

@Temperature 23.0 - 1500 °C
102000 - 131000 psi

@Temperature 73.4 - 2730 °F
UBE Tyrannohex® Heat Resistant Composite
Description: Tyrannohex is a fiber assembled ceramic with both toughness like a shell or wood and excellent heat-resistance in air.Very high volume fraction (Vf) of the thin (~ 10m), continuous fibe..