Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Unnotched | 20.0 J @Temperature 20.0 °C |
14.8 ft-lb @Temperature 68.0 °F |
Transverse |
Industeel CLC 1.2312 Prehardened Mold Steel (300HB/32HRC) with Improved Machinability Description: CLC 1.2312 is a chromium-manganese-molybdenum grade designed for plastic mold industry. This grade is normally delivered in a prehardened condition at a hardness level of 300HB/32HRC. T.. |