Polymer Property : Tear Strength = 94.0 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 94.0 kN/m
536 pli
ASTM D624
C.O.I.M. LARIPUR® LPR2103-90AE PTMG Polyether Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Tear Strength 94.0 kN/m
536 pli
without incision; ISO 34B
Lubrizol ESTANE® 58437 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..