Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 102 - 164 kN/m | 582 - 935 pli | Average value: 136 kN/m Grade Count:6 |
Overview of materials for Ionomer, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma.. |