Polymer Property : Tear Strength = 93.6 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 93.6 kN/m
534 pli
Trouser; ASTM D470
Lubrizol ESTANE® 58149 Ester Based Thermoplastic Polyurethane
Features: Low Compression SetUse: Hydraulic Seals and Gaskets Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.