Polymer Property : Tear Strength = 89.3 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 89.3 kN/m
510 pli
ASTM Die C
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 70A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Tear Strength 89.3 kN/m
510 pli
ASTM Die C
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 70A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..