Polymer Property : Tear Strength = 88.3 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 88.3 kN/m
504 pli
Die C; ASTM D624
SK Chemicals SKYTHANE® 175A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tear Strength 88.3 kN/m
504 pli
Die C; ASTM D624
SK Chemicals SKYTHANE® 870A T series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tear Strength 88.3 kN/m
504 pli
Die C; ASTM D624
SK Chemicals SKYTHANE® CR180A Calendaring Series, Polyether Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tear Strength 88.3 kN/m
504 pli
Die C; ASTM D624
SK Chemicals SKYTHANE® R180A C series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tear Strength 88.3 kN/m
504 pli
Die C; ASTM D624
SK Chemicals SKYTHANE® R180A Polyether Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tear Strength 88.3 kN/m
504 pli
Die C; ASTM D624
SK Chemicals SKYTHANE® T870A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tear Strength 88.3 kN/m
504 pli
Die C; ASTM D624
SK Chemicals SKYTHANE® 180A R series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tear Strength 88.3 kN/m
504 pli
Die C; ASTM D624
SK Chemicals SKYTHANE® S175A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tear Strength 88.3 kN/m
504 pli
Die C; ASTM D624
Lubrizol Estane® S180A Thermoplastic Polyurethane
Type: Estane® S180A is a Shore 83A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: Americas, Europe, Mi..
Tear Strength 88.3 kN/m
504 pli
Die C; ASTM D624
Lubrizol Estane® CR180A Thermoplastic Polyurethane
Type: Estane® CR180A is a Shore 82A, polyether grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf..
Tear Strength 88.3 kN/m
504 pli
Die C; ASTM D624
Lubrizol Estane® CR185A Thermoplastic Polyurethane
Type: Estane® CR185A is a Shore 85A, polyether grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf..