Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 87.5 kN/m | 499 pli | |
Network Polymers Softflex® 7700 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tear Strength | 87.5 kN/m | 499 pli | |
Network Polymers Softflex® 8910 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |