Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 144 kN/m | 820 pli | Die C; ASTM D624 |
Mearthane Durethaneâ„¢ S DS-570D Solid Polyurethane Elastomer TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |