Mechanical Properties Metric English Comments
Tear Strength 81.6 kN/m
466 pli
ASTM D624
Multibase Multi-Flex® TPE D 4308 BLK
The moisture content is 0.04%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength 81.6 kN/m
466 pli
ASTM D624-95
Multibase Multi-Flex® TPO 4308 BLK
Data provided by Multibase.