Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 13.8 kN/m | 79.0 pli | JIS K6301-B |
Stellarchem AB835EM-1 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed unconventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, completel.. |