Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 78.6 kN/m | 448 pli | 78.6 kN/m at 23°C. Value at 100°C is 50.6 kN/m. TPE-0056 (ASTM D 624) |
Advanced Elastomer Systems Santoprene® 253-50 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |