Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 132 kN/m | 753 pli | with incision; ISO 34B |
Lubrizol ESTANE® GP52DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 52DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tear Strength | 132 kN/m | 753 pli | Unnicked; ISO 34-1B |
Lubrizol Estane® GP 52 DT Thermoplastic Polyurethane Type: Estane® GP 52DT is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E.. |