Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 131 kN/m | 747 pli | |
Dow Pellethane® 2102-90AE Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2102-90AE elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with good damping capacity and good hydrolytic sta.. |
|||
Tear Strength | 131 kN/m | 747 pli | ASTM D624 |