Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 72.4 kN/m | 413 pli | Flow; ASTM D624 |
PolyOne Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |