Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 0.877 - 125 kN/m | 5.00 - 713 pli | Average value: 23.8 kN/m Grade Count:694 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |