Polymer Property : Tear Strength = 710 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 124 kN/m
710 pli
Die C; ASTM D624
Mearthane Durethaneâ„¢ S DS-695A Solid Polyurethane Elastomer
MDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..