Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 83.4 - 123 kN/m | 476 - 700 pli | |
Taiwan PU Corporation PPG CPU-1090C Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |