Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 69.9 kN/m | 399 pli | die B; ASTM D624 |
DP7-3002 Polyurethane-based Biomedical Elastomer |
|||
Tear Strength | 69.9 kN/m | 399 pli | Injection molded parts; DIN 53515 |
Huntsman IROGRAN® A 85 H 4508 TPU-Polyester Introduction: IROGRAN A 85 H 4508 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are excellent mechanical properties and hig.. |