Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 116 kN/m | 662 pli | ASTM D624-95 |
Multibase Multi-Flex® TPO D-5016 Multi-Flex® D-5016 is an elastomer modified polypropylene for applications requiring elastomeric properties and good molding behavior.Data provided by Multibase. |
|||
Tear Strength | 116 kN/m | 662 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 5 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 116 kN/m | 662 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 5 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |