Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 107 kN/m | 611 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 4 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 107 kN/m | 611 pli | ASTM D624 |
Kolon ELLAS K-490AB Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon. |
|||
Tear Strength | 107 kN/m | 611 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 4 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |