Mechanical Properties Metric English Comments
Tear Strength 1.14 kN/m
6.50 pli
Average; ASTM D3574
Lendell NolaSponge®
Open CellThis line of foam is furmulated for bath and body sponges. The unique cell structure is ideal for scrubbing and incorporation of bath and soap products.Applications: Bath Sponges, Filtrati..
Tear Strength 1.14 kN/m
6.50 pli
Average; ASTM D3574
Lendell Nolatex® Latex Free Foam
This foam is used in the cosmetics industry and also possesses insulation qualities.Applications:Cosmetic Wedges and Puffs, Padding, High Insulative Value Applications, Makovers ® Disposable Make..
Tear Strength 1.14 kN/m
6.50 pli
Average; ASTM D3574
Lendell Manufacturing HSS Foam
HSS combines the excellent tractile and softness characteristics of Supersoft foams with the strength and durability properties of our Nolatex foams. Strength and softness are key features in this p..