Mechanical Properties Metric English Comments
Tear Strength 6.125 kN/m
34.95 pli
Base Material; ASTM D624
Parker Chomerics CHO-SEAL 1287R Reinforced Conductive Elastomer Seal
These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at..