Polymer Property : Tear Strength = 548 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 96.0 kN/m
548 pli
normal; ISO 34-1
DuPont Performance Polymers Hytrel® 4056P Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer in Powder FormInformation provided by DuPont Performance Polymers