Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 9.47 kN/m | 54.0 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7030-1000 TPE Product Description: StarMediflex P 7030-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
Tear Strength | 9.47 kN/m | 54.0 pli | Die C; ASTM D 624 |
CPT C-Flex® R70-190 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |