Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 500 kN/m
2850 pli
ASTM D624
GRECO ISOTHANE 5085A Polyether TPU Resin
ISOTHANE 5000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility, hydrolytic resistance, fungus resistance, and low temperature performance pro..
Tear Strength 500 kN/m
2860 pli
Initial Tear Strength; ASTM D-1004
Saint-Gobain Norton® Fluorglas® Chemfilm® DF2929 Fluoropolymer Tape
Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super..