Mechanical Properties Metric English Comments
Tear Strength 50.4 kN/m
288 pli
Die C, 510 mm/min; ASTM D624
PolyOne Elastamax™ XL-2085 Thermoplastic Polyolefin Elastomer (TPO (POE))
PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o..