Mechanical Properties Metric English Comments
Tear Strength 85.8 kN/m
490 pli
Die C, 510 mm/min; ASTM D624
PolyOne Elastamax™ EG-9190 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun..
Tear Strength 85.8 kN/m
490 pli
Die C, 510 mm/min; ASTM D624
PolyOne Geon™ Vinyl Flexible A9000 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Tear Strength 85.8 kN/m
490 pli
Die C, 510 mm/min; ASTM D624
PolyOne Geon™ Vinyl Flexible A90U2 Polyvinyl Chloride, Flexible (PVC, Flexible)
GENERAL PURPOSE CLEAR PVC COMPOUND WITH LOW LEVEL OF U.V. INHIBITOR, to be used only in interior applications.Information provided by PolyOne
Tear Strength 85.9 kN/m
490 pli
ASTM D624
Huntsman IROGRAN® A 85 P 4350 TPU-Polyether
Introduction: IROGRAN A 85 P 4350 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th..
Tear Strength 85.9 kN/m
490 pli
ISO 34-1
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tear Strength 85.9 kN/m
490 pli
ISO 34-1
Alliance Polymers Viprene™ G45D-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G45D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..